EN31 Machining, Heat Treatment and Hardening Guide

EN31 Machining

EN31 steel is a high-carbon chromium alloy steel widely used for components that require high hardness, wear resistance and resistance to repeated contact loading. It is commonly selected for bearing components, rollers, shafts, gauges, punches and other precision engineering parts.

However, EN31 does not achieve its final working properties through machining alone. The condition in which the material is supplied, the machining sequence and the heat-treatment process all influence the performance and dimensional accuracy of the finished component.

This guide explains how EN31 round bars are machined, hardened, tempered and finished, along with the important precautions manufacturers and buyers should understand before selecting the material.

1. Understanding the Supplied Condition of EN31 Steel

EN31 is commonly supplied in a spheroidised annealed condition. This condition is intended to make the steel more suitable for machining before final hardening.

In this condition, the material is comparatively softer than its hardened state. It can therefore be turned, drilled, milled and shaped before undergoing the heat-treatment process.

The usual manufacturing sequence is:

  1. Select EN31 material according to the required specification.
  2. Verify the material test certificate and supplied condition.
  3. Carry out rough machining and component shaping.
  4. Perform the specified hardening and tempering treatment.
  5. Finish grind or machine to the required dimensions.
  6. Inspect hardness, dimensions and surface quality.

The exact sequence depends on the component design, machining requirements and final service conditions.

2. Machining of EN31 Round Bar

Machining EN31 is generally easier when the material is supplied in a suitable annealed condition. Its high carbon and chromium content means that machining becomes considerably more demanding after hardening.

Turning

Turning is commonly used to produce cylindrical components such as bearing-related parts, rollers, pins and shafts.

For better machining results:

  • Prefer machining in the annealed condition.
  • Select cutting tools suitable for the material condition.
  • Use appropriate cutting speeds and feeds.
  • Maintain effective cutting-fluid application where required.
  • Avoid excessive heat during machining.

Milling and Drilling

Milling and drilling may be used to create slots, holes, grooves and other component features before hardening.

The machining method should account for the material’s high carbon content. Tool selection, cutting parameters and workpiece stability are important to prevent excessive tool wear and poor surface finish.

Machining Before Hardening

Where the component design permits, most material removal is generally completed before hardening.

This approach helps reduce machining difficulty and tool wear. However, the component should not necessarily be machined to its final dimensions before heat treatment because hardening can cause dimensional changes.

A suitable finishing allowance should be considered where subsequent grinding is required.

3. EN31 Heat Treatment Process

Heat treatment changes the microstructure and hardness of EN31 steel. It is used to achieve the properties required for the component’s operating conditions.

The principal processes include annealing, hardening and tempering.

A. Annealing

Annealing is used to soften the steel and improve its suitability for machining.

EN31 is commonly supplied in a spheroidised annealed condition. Spheroidisation helps produce a structure suitable for machining before the final hardening operation.

If material has undergone forging or a previous heat-treatment operation, the appropriate annealing procedure should be selected according to its condition and the applicable material specification.

B. Hardening

Hardening increases the hardness and wear resistance of EN31.

For reference, published technical information for 100Cr6 bearing steel describes hardening temperatures in the approximate range of 830–870°C, followed by oil quenching. Other EN31/535A99 references may specify different working ranges.

During hardening, the steel is heated to the specified temperature, held for the required period and then cooled using the selected quenching method.

The correct process depends on:

  • Actual grade and material specification
  • Component dimensions and cross-section
  • Furnace temperature uniformity
  • Required hardness
  • Quenching equipment and medium
  • Component geometry

An incorrect hardening cycle can result in cracking, distortion or inconsistent hardness.

C. Quenching

Quenching is the rapid cooling stage following hardening.

Oil quenching is commonly specified for 100Cr6-type bearing steel. The cooling process transforms the steel’s microstructure and develops high hardness.

The quenching method must be selected carefully because the rapid temperature change can produce internal stresses.

Components with sharp corners, abrupt section changes or uneven thickness may be particularly sensitive to distortion and cracking.

D. Tempering

Tempering is carried out after hardening to reduce excessive brittleness and improve the balance between hardness and toughness.

For bearing applications, published 100Cr6 heat-treatment guidance commonly refers to low-temperature tempering, with examples around 150–200°C depending on the required properties and specification.

Tempering should follow hardening promptly. Ovako’s 100Cr6 guidance specifies tempering within two hours after oil quenching, at a minimum temperature of 160°C.

The selected tempering temperature affects the final hardness. Therefore, the heat-treatment cycle must be chosen according to the component’s intended application rather than relying on one temperature for every EN31 part.

4. Typical EN31 Heat Treatment Reference

The following table provides general reference information drawn from published 100Cr6 and EN31-related technical guidance.

ProcessPublished reference information
Supplied conditionCommonly spheroidised annealed
Hardening temperatureApproximately 830–870°C in published 100Cr6 guidance
QuenchingOil quenching is commonly specified
TemperingCommonly low-temperature tempering for bearing applications
Tempering timingPromptly after quenching; Ovako specifies within two hours
Final hardnessDepends on specification, treatment and component section

Important: These are reference values, not a universal heat-treatment recipe or a guaranteed EN31 property range. EN31, 535A99 and 100Cr6 designations must be checked against the actual material specification and test certificate. A qualified heat-treatment specialist should determine the final cycle for the component.

For further technical reference, consult Ovako’s 100Cr6 steel grade and heat-treatment guidance and the Hillfoot 535A99 material datasheet.

5. EN31 Hardness After Heat Treatment

One of the main reasons EN31 is selected for engineering applications is its ability to achieve high hardness after suitable heat treatment.

Hardened 100Cr6-type bearing steel is commonly associated with hardness around 60–64 HRC under suitable treatment conditions. However, the actual result depends on the grade specification, component section, quenching conditions and tempering cycle.

Hardness should always be verified against the required component specification.

For buyers, it is important to distinguish between:

  • Hardness in the supplied annealed condition
  • Hardness after hardening
  • Final hardness after tempering
  • Surface hardness and core hardness, where relevant

A material certificate for an annealed round bar should not be treated as proof of the hardness that will be achieved after the customer’s heat-treatment process.

6. Grinding and Finishing EN31 Components

Grinding is frequently used after hardening to achieve the dimensional accuracy and surface finish required for precision components.

This is particularly important for bearing-related applications, where dimensional accuracy and surface quality can influence performance.

Common finishing operations include:

  • Cylindrical grinding
  • Surface grinding
  • Internal grinding
  • Precision dimensional finishing

Why Grinding Allowance Matters

Heat treatment can cause dimensional changes due to thermal expansion, phase transformation and residual stresses.

For this reason, manufacturers should consider suitable grinding allowance during the initial machining stage.

The required allowance depends on component size, geometry, heat-treatment conditions and the expected dimensional movement.

Avoiding Grinding Damage

Excessive grinding heat can damage the surface of hardened steel. Grinding parameters, wheel selection, dressing and cooling arrangements should be controlled to avoid surface burns, cracks and unwanted changes in hardness.

Final inspection should include the relevant dimensional and surface-quality checks.

7. Common Problems During EN31 Heat Treatment

Incorrect processing can affect the reliability and accuracy of EN31 components.

Distortion

Uneven heating or cooling, component geometry and residual stresses can cause dimensional changes during hardening.

Precaution: Plan the machining sequence and finishing allowance around the expected heat-treatment movement.

Quenching Cracks

Rapid cooling can create high internal stresses. Sharp corners and abrupt changes in section can increase the risk.

Precaution: Use a suitable component design and a controlled heat-treatment procedure.

Inconsistent Hardness

Incorrect heating, inadequate soaking or uneven quenching can result in inconsistent hardness.

Precaution: Ensure proper furnace control and verify hardness at appropriate inspection locations.

Grinding Burns

Excessive heat during grinding can damage the hardened surface.

Precaution: Use suitable grinding parameters and effective cooling.

Excessive Brittleness

A hardened component that has not been tempered appropriately may have an unsuitable balance of hardness and toughness.

Precaution: Follow the specified tempering cycle and verify the final properties.

8. Is EN31 Suitable for Welding?

EN31 is a high-carbon chromium steel and is generally not selected for conventional welding applications.

Its high carbon content and hardenability make welding difficult. Local heating and cooling can create hard microstructures, residual stresses and cracking risks.

Where a component requires welding, the material selection and joining procedure should be reviewed by a qualified welding specialist.

For components involving significant welding or fabrication, an alternative steel grade may be more appropriate depending on the required strength, toughness and service conditions.

9. Applications That Require EN31 Hardening

EN31 is used in components where high hardness and wear resistance are important.

Typical applications include:

  • Ball and roller bearing components
  • Bearing rings and races
  • Precision rollers
  • Lathe centres
  • Collets
  • Cams and pawls
  • Gauges and measuring components
  • Punches and selected tooling
  • Instrument pivots and spindles

The final suitability of EN31 depends on the operating load, contact conditions, component geometry and heat-treatment quality.

It is particularly important to assess the material carefully where the component is exposed to heavy impact or shock loading, because high hardness does not automatically mean high impact toughness.

10. What Buyers Should Check Before Purchasing EN31 Round Bar

Selecting the correct material before machining and heat treatment can help avoid costly production issues.

Buyers and engineering teams should confirm the following:

  1. Material designation: Confirm whether the requirement is EN31, 535A99, 100Cr6 or another specified grade.
  2. Dimensions: Confirm the required diameter, length and dimensional tolerance.
  3. Supply condition: Check whether the material is required in an annealed or another specified condition.
  4. Material test certificate: Verify the chemical composition and applicable specification.
  5. Heat-treatment requirement: Clarify whether the buyer requires untreated material or a heat-treated product.
  6. Hardness requirement: Specify the required hardness and testing method, where applicable.
  7. Final application: Share the intended component and operating conditions to help confirm material suitability.

Buyers should not assume that different grade designations are automatically interchangeable. The actual specification and material certificate should be checked before production.

For dimensional planning, buyers can also refer to the Manan Steel & Metals round bar weight chart.

11. EN31 Round Bar Supply from Manan Steel & Metals

Manan Steel & Metals deals in specialty metals, alloy steels and stainless steel products for industrial and engineering requirements.

EN31 round bars can be considered for applications involving bearing components, precision engineering parts, wear-resistant components and other suitable industrial uses.

When enquiring, buyers are requested to share:

  • Required EN31 diameter
  • Required length or quantity
  • Applicable grade or specification
  • Required supply condition
  • Material test certificate requirements
  • Intended application, where relevant

Material specifications and availability should be confirmed at the time of enquiry.

For EN31 round bar enquiries, contact:

Manan Steel & Metals
Established: 2007
Mumbai, Maharashtra, India

Website: https://manansteel.com/
Email: sales@manansteel.com
Phone: +91 98198 76962

Contact Manan Steel & Metals for EN31 Round Bar Enquiries

Frequently Asked Questions About EN31 Machining and Heat Treatment

1. Is EN31 easy to machine?

EN31 is comparatively easier to machine in its spheroidised annealed condition. Machining becomes more difficult after hardening because of the increased hardness.

2. Does EN31 require heat treatment?

For applications requiring high hardness and wear resistance, EN31 is generally hardened and tempered after machining. The exact requirement depends on the component and its intended use.

3. What is the hardening temperature of EN31?

Published 100Cr6 bearing-steel guidance commonly gives a hardening range around 830–870°C. The correct temperature must be selected according to the actual grade specification and heat-treatment procedure.

4. Is EN31 oil quenched?

Oil quenching is commonly specified for 100Cr6-type bearing steel. The appropriate quenching method depends on the material specification, section size and component geometry.

5. What hardness can EN31 achieve?

Suitable hardened 100Cr6-type material can achieve approximately 60–64 HRC. Actual hardness depends on the material and the complete heat-treatment cycle.

6. Can EN31 be machined after hardening?

Conventional machining becomes considerably more difficult after hardening. Grinding is commonly used for final dimensional finishing of hardened EN31 components.

7. Can EN31 be welded?

EN31 is generally not recommended for conventional welding because of its high carbon content and risk of cracking. A qualified specialist should assess any proposed joining procedure.

8. Why is grinding required after EN31 hardening?

Grinding helps achieve the required dimensional accuracy and surface finish after heat treatment. It also allows manufacturers to account for dimensional changes during hardening.

Conclusion

EN31 is a high-carbon chromium steel used in applications requiring high hardness and wear resistance. Its performance depends not only on the material grade but also on the supplied condition, machining sequence, hardening, tempering and final finishing operations.

For buyers and manufacturers, understanding these stages helps in selecting the correct EN31 round bar and planning the production process more effectively.

For EN31 round bar requirements, contact Manan Steel & Metals with your required grade, dimensions, quantity and material specification.