Alloy A286 round bar is a high-performance iron-nickel-chromium alloy developed for engineering applications that require high strength, oxidation resistance and reliable performance at elevated temperatures. Also identified as UNS S66286, A286 is an age-hardenable alloy used in aerospace components, high-temperature fasteners, turbine equipment, automotive engineering and specialised industrial applications.
Known by designations such as A286, Incoloy A-286 and Grade 660 in certain specifications, this alloy offers a combination of mechanical strength and temperature capability that makes it useful for demanding engineering requirements.
For buyers, selecting the correct A286 round bar involves understanding its material properties, heat-treatment condition, applicable standards, dimensions and documentation.
This guide explains the essential information industrial purchasers and engineers should know before sourcing Alloy A286 round bars.
Table of Contents
ToggleAlloy A286 is an age-hardenable iron-nickel-chromium alloy containing additions of titanium and molybdenum, along with other alloying elements.
Its strengthening mechanism involves precipitation hardening. This allows the alloy to achieve high mechanical strength after the appropriate solution-treatment and ageing process.
Important material designations include:
| Designation | Description |
|---|---|
| Alloy A286 | Common commercial alloy name |
| Incoloy A-286 | Common trade designation |
| UNS S66286 | Unified Numbering System designation |
| Grade 660 | Designation used in certain specifications |
| W.Nr. 1.4980 | Common European material number |
These designations are useful when searching for or specifying the material. However, buyers should confirm the exact specification, product form and condition because similar designations do not automatically establish compliance with every purchasing requirement.
The chemical composition of A286 is designed to provide high-temperature strength, oxidation resistance and age-hardening capability.
The principal alloying elements include nickel, chromium, titanium and molybdenum.
Typical specification limits include:
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | 24.00–27.00 |
| Chromium (Cr) | 13.50–16.00 |
| Titanium (Ti) | 1.90–2.35 |
| Molybdenum (Mo) | 1.00–1.50 |
| Vanadium (V) | 0.10–0.50 |
| Boron (B) | 0.003–0.010 |
| Carbon (C) | 0.08 maximum |
| Manganese (Mn) | 2.00 maximum |
| Silicon (Si) | 1.00 maximum |
| Aluminium (Al) | 0.35 maximum |
| Iron (Fe) | Balance |
The exact permitted limits depend on the governing specification and product requirements. Always verify the chemical analysis against the applicable standard and material test certificate.
Nickel: Helps maintain the austenitic structure and contributes to the alloy’s high-temperature properties.
Chromium: Contributes to oxidation and corrosion resistance.
Titanium: Plays an important role in precipitation hardening and strength development.
Molybdenum: Contributes to strength and mechanical performance.
Vanadium and boron: Help support the alloy’s strengthening and metallurgical characteristics.
Mechanical properties are an important consideration when selecting A286 round bars for high-strength engineering components.
The properties of A286 vary according to the product specification, section size, solution-treatment condition and ageing process.
In an aged condition, certain A286 product specifications provide minimum tensile strength values around 965 MPa and minimum yield strength around 655 MPa. These values are not universal guarantees for every bar or product condition.
The following properties should be checked before purchase:
A286 is precipitation hardenable. Its final mechanical properties depend significantly on the specified heat-treatment process.
Solution treatment and subsequent ageing are used to develop the required properties.
Buyers should therefore avoid comparing mechanical-property figures without checking whether the materials are in the same heat-treatment condition and covered by the same product specification.
For detailed technical information, refer to the ATI A286 Technical Data Sheet.
The physical properties of A286 are relevant when engineers evaluate weight, thermal expansion, operating temperature and component design.
Some reference properties include:
| Property | Approximate value |
|---|---|
| Density | 7.94–7.98 g/cm³ |
| Melting range | Approximately 1,371–1,427°C |
| Material family | Iron-nickel-chromium alloy |
| Strengthening mechanism | Precipitation hardening |
These values are reference information. Actual material data should be checked against the selected product specification and manufacturer’s technical documentation.
One of the main reasons A286 is selected for engineering applications is its ability to retain useful strength at elevated temperatures.
The alloy has been used in applications requiring high strength and corrosion resistance at temperatures up to approximately 704°C, depending on the component design, loading conditions and environment.
It also offers oxidation resistance at elevated temperatures.
Applications involving high temperatures must be evaluated carefully. The maximum suitable service temperature is not a universal design limit because actual performance depends on:
Engineers should use approved material data and design allowables rather than relying only on general temperature descriptions.
A286 provides useful oxidation resistance and corrosion performance in selected environments.
Its chromium content contributes to the formation of a protective surface oxide layer. The alloy is used in applications where a combination of mechanical strength and environmental resistance is required.
However, A286 should not be treated as universally corrosion-proof.
Before selecting the alloy, consider:
The material’s suitability should be confirmed against the actual service conditions.
A286 round bars are used as raw material for manufacturing components that require high strength and elevated-temperature performance.
A286 is used in selected aerospace applications, including engine hardware, fasteners and other components requiring high mechanical strength.
The alloy is used in selected turbine-related components exposed to elevated temperatures and mechanical stresses.
A286 is an important material for specialised bolts, nuts, studs and other fasteners used in demanding operating environments.
Selected high-performance automotive components and supercharger-related applications use A286 where its mechanical and temperature properties are appropriate.
A286 can be used for shafts, machined parts, specialised fittings and other engineered components where the specified properties are required.
The alloy is also used in certain spring and precision engineering applications, depending on the required condition and product specification.
The applicable specification depends on the product form and intended application.
For A286, buyers may encounter several AMS and ASTM specifications.
Examples include:
| Specification | General product scope |
|---|---|
| AMS 5731 | Bars, rings, forgings and tubing |
| AMS 5732 | Bars, rings, forgings and tubing |
| AMS 5734 | Bars, rings, forgings and tubing |
| AMS 5737 | Bars, rings, forgings and tubing |
| ASTM A638 | Precipitation-hardening iron-base superalloy bars, forgings and forging stock |
| ASTM A453 | High-temperature bolting materials |
These standards are not interchangeable. The correct specification must be selected according to the product form, required heat treatment and application.
For bar requirements, the buyer should confirm the precise AMS or ASTM specification rather than simply requesting A286 material.
Refer to the ATI A286 product information and technical documents for manufacturer information and product-specific documentation.
Before placing an order, industrial buyers should provide the supplier with complete technical details.
Confirm Alloy A286 / UNS S66286 and any additional designation required by the project.
Specify the required round bar diameter and length, including any cutting or machining allowance.
Mention the required AMS or ASTM specification and edition, where specified.
State whether the material must be supplied solution treated, aged or in another specified condition.
Confirm the required tensile strength, yield strength, hardness and elongation for the ordered product.
Specify whether an MTC, heat-number traceability or additional inspection reports are required.
Mention the number of pieces or required weight and the delivery location.
Providing these details helps the supplier review the requirement accurately and respond with relevant sourcing information.
Manan Steel & Metals, established in 2007, deals in specialty metals and alloy products for industrial requirements.
The product range includes Alloy A286 and other specialty materials such as Inconel, Monel, Invar, Titanium, Nitronic and engineering alloys.
For Alloy A286 round bar enquiries, buyers can share the required diameter, length, quantity, material specification and documentation requirements.
The requirement can then be reviewed for sourcing and availability confirmation.
Contact Manan Steel & Metals
For product enquiries, visit the Manan Steel & Metals Contact Page.
The UNS designation for Alloy A286 is S66286.
A286 and Incoloy A-286 are commonly used names for the same alloy family. However, the applicable product specification and material condition must still be confirmed.
Yes. A286 is a precipitation-hardening alloy. Its mechanical strength can be increased through the appropriate solution-treatment and ageing process.
Depending on the ordered product and requirements, specifications may include AMS 5731, AMS 5732, AMS 5734, AMS 5737 and ASTM A638. Confirm the exact specification with the purchase requirement.
A286 is used in selected high-temperature applications requiring strength and oxidation resistance. Actual suitability depends on temperature, loading, exposure duration and engineering design requirements.
Yes. A286 is used for specialised fasteners such as bolts, studs and other components requiring high strength and elevated-temperature performance.
A286 is precipitation hardenable. The required solution-treatment and ageing condition depends on the product specification and application.
Provide the grade, UNS number, diameter, length, quantity, applicable specification, heat-treatment condition and required inspection documentation.
Alloy A286 round bar is an important engineering material for applications requiring high mechanical strength, oxidation resistance and performance at elevated temperatures.
Its precipitation-hardening characteristics, nickel-chromium composition and specialised product specifications make correct material selection particularly important.
For buyers, confirming the grade, product specification, dimensions, heat-treatment condition and material documentation before purchase helps ensure that the supplied material matches the engineering requirement.
For Alloy A286 round bar enquiries, contact Manan Steel & Metals with your required dimensions, quantity and specification details.
SEO Title: Alloy A286 Round Bar: Properties, Specifications & Uses
Focus Keyword: Alloy A286 round bar
Secondary Keywords:
URL Slug: alloy-a286-round-bar-properties-specifications-uses
Meta Description: Explore Alloy A286 round bar properties, UNS S66286 specifications, heat treatment, high-temperature performance and industrial applications.
Featured Image Filename: alloy-a286-round-bar-uns-s66286.jpg
Featured Image Alt Text: Alloy A286 UNS S66286 high temperature alloy round bar
Featured Image Caption: Alloy A286 round bars for high-strength industrial and high-temperature engineering applications.
Internal Links Included:
External Follow Links Included:
Publishing Checklist: