Alloy A286 Chemical Composition
Alloy A286 is an age-hardenable iron-nickel-chromium alloy developed for engineering applications requiring high mechanical strength, oxidation resistance and dependable performance at elevated temperatures. Identified by UNS S66286, it is used in aerospace components, gas turbines, high-temperature fasteners and specialised industrial equipment.
One of the most important characteristics of A286 is its ability to develop higher strength through controlled solution treatment and precipitation ageing. Its final mechanical properties depend on the chemical composition, product form, heat-treatment cycle and applicable material specification.
For engineers and industrial buyers, understanding the chemical composition, tensile strength, yield strength, hardness and heat-treatment condition is essential when selecting Alloy A286.
Table of Contents
ToggleA286 is an iron-based, austenitic precipitation-hardening alloy. Its composition includes nickel, chromium, titanium and molybdenum, with smaller controlled additions of elements such as vanadium, boron and aluminium.
The combination of these elements contributes to its strength, oxidation resistance and high-temperature performance.
| Element | Composition by weight (%) |
|---|---|
| Nickel (Ni) | 24.00–27.00 |
| Chromium (Cr) | 13.50–16.00 |
| Titanium (Ti) | 1.90–2.35 |
| Molybdenum (Mo) | 1.00–1.50 |
| Vanadium (V) | 0.10–0.50 |
| Manganese (Mn) | 2.00 maximum |
| Silicon (Si) | 1.00 maximum |
| Aluminium (Al) | 0.35 maximum |
| Carbon (C) | 0.08 maximum |
| Cobalt (Co) | 1.00 maximum |
| Phosphorus (P) | 0.025 maximum |
| Sulphur (S) | 0.015 maximum |
| Boron (B) | 0.003–0.010 |
| Iron (Fe) | Balance |
These are composition limits published in ATI’s technical information. The governing product specification and its applicable edition must be checked before accepting a material. The limits may differ between specifications or product requirements.
Nickel (Ni)
Nickel helps maintain the austenitic structure and contributes to the alloy’s mechanical properties and performance at elevated temperatures.
Chromium (Cr)
Chromium contributes to oxidation resistance by supporting the formation of a protective oxide layer on the material surface.
Titanium (Ti)
Titanium is an important strengthening addition. It participates in the precipitation-hardening mechanism that helps A286 achieve higher strength after ageing.
Molybdenum (Mo)
Molybdenum contributes to the alloy’s strength and high-temperature mechanical performance.
Vanadium (V)
Vanadium is a controlled alloying addition that contributes to the material’s metallurgical characteristics.
Boron (B)
Boron is present in a small controlled amount and contributes to the alloy’s grain-boundary and high-temperature properties.
A286 is strengthened through precipitation hardening, also known as age hardening.
The process involves two important stages:
During solution treatment, the material is heated to a specified temperature so that the alloying elements required for strengthening are brought into solid solution.
The material is then cooled according to the applicable procedure. Subsequent ageing allows strengthening precipitates to develop within the alloy’s microstructure.
These precipitates restrict dislocation movement and increase the material’s strength and hardness.
The exact heat-treatment procedure depends on the ordered specification and the required properties.
Mechanical properties are among the most important factors when selecting A286 for high-strength engineering applications.
The material’s tensile strength, yield strength, elongation and hardness vary according to its product form and heat-treatment condition.
For example, ATI’s published product information for precipitation-heat-treated sheet and plate under AMS 5525 lists the following minimum mechanical properties:
| Property | Published requirement |
|---|---|
| Tensile strength | 965 MPa minimum |
| Yield strength | 655 MPa minimum |
| Elongation | 15% minimum |
| Hardness | 24–35 HRC |
Important: These values refer to the specified sheet and plate product requirements. They must not automatically be applied to every A286 round bar. Bar properties should be checked against the applicable bar specification, such as the relevant AMS 5731, 5732, 5734 or 5737 requirement.
Tensile strength indicates the maximum stress a material can withstand while being stretched before fracture.
A286 is used in components requiring high tensile strength, particularly after the specified precipitation-hardening treatment.
Yield strength indicates the stress at which permanent deformation begins under the defined test conditions.
It is an important design consideration for fasteners, shafts, turbine components and other load-bearing parts.
Elongation measures the material’s ability to deform plastically before fracture.
The required elongation depends on the product specification, material condition and test requirements.
Hardness indicates resistance to local indentation or surface deformation.
A286 hardness increases after suitable precipitation ageing. The required hardness range should always be checked against the applicable product specification and heat-treatment condition.
Heat treatment is central to achieving the required properties of A286.
The two principal stages are solution treatment and precipitation ageing.
ATI’s technical data describes two solution-treatment routes for A286:
| Solution-treatment route | Temperature | Holding time |
|---|---|---|
| Lower-temperature route | 899°C (1650°F) | 2 hours |
| Higher-temperature route | 982°C (1800°F) | 1 hour |
The appropriate cooling method and process details must follow the governing material specification and approved heat-treatment procedure.
The choice between these routes depends on the required balance of mechanical properties, ductility and high-temperature performance.
After solution treatment, the material is aged to develop the required strength.
ATI’s technical data identifies an ageing range of:
The exact cycle must be selected according to the applicable specification and product condition. The time, temperature and cooling requirements should not be changed without engineering approval.
Different solution-treatment routes are specified because the resulting properties can vary.
For example, ATI describes the 1650°F and 1800°F solution-treatment routes in relation to different combinations of tensile, yield, creep and stress-rupture performance.
The correct route should therefore be selected according to the application and the governing specification, rather than assuming that one heat-treatment cycle is suitable for every A286 component.
Hardness is influenced by the material’s condition and the precipitation-hardening process.
ATI’s technical information provides the following reference ranges:
| Material condition | Brinell hardness |
|---|---|
| Solution treated | Approximately 140–180 HB |
| After ageing | Approximately 248–321 HB |
These are reference values from the cited technical information. Actual acceptance requirements depend on the product specification, heat-treatment route and ordered condition.
For industrial procurement, the buyer should specify the required hardness test method and acceptance range where hardness is a contractual requirement.
A286 is used in applications where mechanical strength must be maintained at elevated temperatures.
ATI identifies applications requiring high strength and corrosion resistance up to approximately 704°C (1300°F).
The alloy is also used in certain cryogenic applications.
However, mechanical properties change with temperature. Tensile strength, yield strength, creep resistance and stress-rupture performance must be evaluated at the actual service temperature.
When specifying A286 for high-temperature equipment, engineers should consider:
Room-temperature tensile properties alone are not sufficient to establish suitability for a high-temperature component.
A286 combines useful oxidation resistance with corrosion performance in selected industrial environments.
Its chromium content contributes to oxidation resistance at elevated temperatures, while its nickel content supports its austenitic alloy structure.
ATI reports oxidation resistance up to approximately 982°C (1800°F) under specified test and exposure conditions.
This should not be confused with a universal recommended continuous service temperature. Oxidation performance and mechanical strength are different considerations.
For component selection, the following factors should be evaluated:
The alloy should be approved for the actual service environment before being selected for critical equipment.
A286 is supplied under different specifications depending on its product form and required condition.
Examples of relevant AMS specifications include:
| Specification | General product scope or condition |
|---|---|
| AMS 5731 | Bars, rings, forgings and tubing – 1800°F solution treatment |
| AMS 5732 | Bars, rings, forgings and tubing – 1800°F solution treatment and ageing |
| AMS 5734 | Bars, rings, forgings and tubing – 1650°F solution treatment |
| AMS 5737 | Bars, rings, forgings and tubing – 1650°F solution treatment and ageing |
| AMS 5525 | Sheet, strip and plate |
| ASTM A638 | Precipitation-hardening iron-base superalloy bars, forgings and forging stock |
The specification must match the ordered product form. For example, sheet and plate requirements should not be used as a substitute for bar requirements.
Refer to the ATI A286 Technical Data Sheet and ATI A286 Product Information for manufacturer-published information.
A Material Test Certificate (MTC) provides important information for verifying the supplied material against the purchase order.
For A286 round bars, buyers should review:
The certificate should be checked against the actual specification and the ordered material condition.
If the component requires a specific aged condition, confirm that the supplied documentation demonstrates compliance with that requirement.
Two materials carrying the same A286 grade designation may have different mechanical properties if they are supplied under different specifications or heat-treatment conditions.
This is why buyers should avoid selecting A286 based only on the grade name.
Before placing an order, confirm:
These details help prevent misunderstandings between the buyer, supplier and end user.
Manan Steel & Metals, established in 2007, deals in specialty metals and alloy products for industrial requirements.
The product range includes Alloy A286 and other specialty materials such as Inconel, Monel, Invar, Titanium, Nitronic and engineering alloys.
For Alloy A286 round bar enquiries, buyers can share the required diameter, length, quantity, specification and heat-treatment condition.
Material documentation and availability requirements can be reviewed against the enquiry.
Contact Manan Steel & Metals
For product enquiries, visit the Manan Steel & Metals Contact Page.
A286 contains approximately 24–27% nickel, 13.5–16% chromium, 1.9–2.35% titanium and 1–1.5% molybdenum, with iron as the balance. The exact limits must be checked against the applicable product specification.
Yes. A286 is an age-hardenable alloy. Its strength is increased through solution treatment followed by controlled precipitation ageing.
ATI describes solution-treatment routes at approximately 899°C (1650°F) and 982°C (1800°F), followed by ageing in the range of approximately 704–760°C (1300–1400°F). The selected cycle must follow the ordered specification.
The tensile strength depends on product form and heat-treatment condition. ATI lists a minimum tensile strength of 965 MPa for certain precipitation-heat-treated sheet and plate requirements under AMS 5525. Bar requirements must be checked against the applicable bar specification.
ATI’s technical information gives an approximate aged hardness range of 248–321 HB for the described heat-treatment condition. The actual acceptance range depends on the governing specification.
Solution-treated A286 has undergone the solution-treatment stage. Aged A286 has also undergone precipitation heat treatment to develop higher strength and hardness.
Titanium is a key strengthening addition. It participates in the precipitation-hardening mechanism that develops higher strength after the specified heat-treatment process.
Yes. A286 is used in selected high-temperature applications requiring mechanical strength and oxidation resistance. Actual suitability depends on the operating temperature, loading, exposure duration and design requirements.
Alloy A286 is a specialised engineering alloy whose performance depends on both its chemical composition and heat-treatment condition.
Nickel, chromium, titanium and molybdenum contribute to its material characteristics, while controlled solution treatment and precipitation ageing help develop the required strength and hardness.
For industrial buyers, verifying the product specification, material condition, mechanical test results and MTC is essential before purchasing A286 round bars.
For Alloy A286 round bar requirements, contact Manan Steel & Metals with your required dimensions, quantity and specification details.
SEO Title: Alloy A286 Chemical Composition, Properties & Heat Treatment
Focus Keyword: Alloy A286 chemical composition
Secondary Keywords:
URL Slug: alloy-a286-chemical-composition-mechanical-properties-heat-treatment
Meta Description: Learn Alloy A286 chemical composition, mechanical properties, hardness and solution treatment and ageing requirements for industrial applications.
Featured Image Filename: alloy-a286-chemical-composition-heat-treatment.jpg
Featured Image Alt Text: Alloy A286 UNS S66286 chemical composition and heat treatment
Featured Image Caption: Alloy A286 composition and precipitation-hardening process for high-strength engineering applications.
Internal Links Included:
External Follow Links Included:
Publishing Checklist: