Hastelloy C276 Chemical Composition, Mechanical Properties and Corrosion Resistance

Focus keyword: Hastelloy C276 chemical composition
URL slug: hastelloy-c276-chemical-composition-mechanical-properties-corrosion-resistance

Hastelloy C276 Chemical Composition

Hastelloy C276 is a nickel-based corrosion-resistant alloy developed for industrial environments involving aggressive chemicals, acids and chloride-bearing solutions. Identified by UNS N10276 and Werkstoff Number 2.4819, it is widely used in chemical processing, pollution control, pharmaceutical production and other demanding industries.

The performance of Hastelloy C276 is closely connected to its chemical composition, particularly its nickel, chromium, molybdenum and tungsten content. These elements contribute to its resistance to different forms of corrosion, including pitting, crevice corrosion and stress corrosion cracking.

Understanding Hastelloy C276 chemical composition, mechanical properties and corrosion resistance helps engineers, procurement teams and industrial buyers evaluate the alloy for their applications.

1. What Makes Hastelloy C276 a Corrosion-Resistant Alloy?

Hastelloy C276 belongs to the nickel-chromium-molybdenum family of corrosion-resistant alloys. It also contains tungsten, iron and controlled quantities of other elements.

Its composition is designed to provide resistance in a wide range of chemical environments, including selected oxidizing and reducing conditions.

The alloy is particularly known for:

  • Resistance to many aggressive chemical environments
  • Good resistance to chloride-induced pitting and crevice corrosion
  • Resistance to chloride-related stress corrosion cracking
  • Resistance to selected oxidizing and non-oxidizing acids
  • Good weldability and fabricability
  • Low carbon and silicon content

Hastelloy is a registered trademark of Haynes International. C276 is also commonly described as Alloy C276 or UNS N10276.

2. Hastelloy C276 Chemical Composition

The chemical composition of Hastelloy C276 determines many of its corrosion-resistant characteristics.

The following table shows commonly specified composition ranges and maximum limits. Actual requirements should be checked against the applicable product specification and Material Test Certificate (MTC).

ElementComposition (weight %)
NickelBalance
Chromium14.5–16.5
Molybdenum15.0–17.0
Iron4.0–7.0
Tungsten3.0–4.5
Cobalt2.5 max
Manganese1.0 max
Vanadium0.35 max
Silicon0.08 max
Carbon0.01 max
Phosphorus0.04 max
Sulfur0.03 max

Role of the Main Alloying Elements

Nickel

Nickel forms the balance of the alloy and provides the base for its corrosion-resistant performance in many aggressive environments.

Chromium

Chromium contributes to resistance in oxidizing environments and supports the formation of a protective surface film.

Molybdenum

Molybdenum is an important contributor to resistance against localized corrosion, particularly pitting and crevice attack in chloride-bearing environments.

Tungsten

Tungsten contributes to the alloy’s resistance in selected aggressive chemical conditions and works alongside molybdenum and chromium.

Iron

Iron is present as a significant alloying constituent and forms part of the overall composition balance.

Low carbon and silicon

The controlled low levels of carbon and silicon help reduce concerns about unwanted precipitation during welding and support the alloy’s suitability for fabricated equipment.

3. Hastelloy C276 Mechanical Properties

Hastelloy C276 combines useful strength with ductility and can be fabricated using appropriate industrial processes.

Its mechanical properties depend on several factors, including:

  • Product form
  • Diameter or thickness
  • Heat-treatment condition
  • Degree of cold working
  • Applicable material specification
  • Testing method

Tensile and yield properties

Tensile strength measures the maximum stress a material withstands during a tensile test before fracture. Yield strength indicates the stress at which permanent deformation begins under the specified test method.

For C276, these values should be taken from the relevant product specification and certified test results.

Haynes International publishes mechanical test data for different product forms. For example, its published room-temperature data for mill-annealed sheet show approximately:

PropertyPublished sheet value
0.2% offset yield strength356 MPa
Ultimate tensile strength792 MPa
Elongation61%

Important: These are published values for a specific sheet thickness and condition, not guaranteed values for every C276 round bar or product form. Buyers should use the actual MTC and applicable bar specification for design and acceptance.

Hardness

Hardness is influenced by the material’s condition and degree of cold working.

Haynes International publishes a typical Rockwell B hardness value of 86 for solution-annealed bar. The actual supplied material should be verified against its specification and test documentation.

Ductility and workability

C276 has useful ductility and can be formed using suitable fabrication procedures. It also work hardens during cold working, which should be considered when planning machining and forming operations.

4. Physical Properties of Hastelloy C276

Physical properties are relevant when designing components, calculating material requirements and evaluating performance under operating conditions.

Commonly published reference values include:

Physical propertyApproximate value
Density8.89 g/cm³
Modulus of elasticity205 GPa
Thermal conductivity10.5 W/m·K at 50°C
Melting range1323–1371°C
Coefficient of thermal expansion11.2 µm/m·°C (24–100°C)

These are reference values. Physical properties can vary with temperature and testing conditions.

5. Hastelloy C276 Corrosion Resistance

Corrosion resistance is one of the main reasons industries select Hastelloy C276.

Its chromium and molybdenum content, together with other alloying elements, provides resistance to several aggressive chemical environments.

However, corrosion performance must always be evaluated according to the actual chemical concentration, temperature, contaminants, flow conditions and exposure duration.

Resistance to hydrochloric acid

C276 is used in selected hydrochloric-acid environments because it offers stronger resistance than many conventional stainless steels under certain conditions.

Haynes International’s comparative corrosion information demonstrates the alloy’s advantage over 316L and 254SMO in specified hydrochloric-acid test conditions.

This does not mean that C276 is immune to hydrochloric acid attack at every concentration or temperature.

Resistance to sulfuric acid

The alloy is also used in selected sulfuric-acid processing environments.

Its performance depends on acid concentration, temperature and the presence of impurities or other chemicals.

Resistance to pitting and crevice corrosion

Pitting and crevice corrosion are localized forms of attack that can damage equipment even when the general surface appears relatively unaffected.

C276 offers high resistance to chloride-induced pitting and crevice corrosion. This is particularly relevant for components used in chemical processing and selected marine or pollution-control applications.

Resistance to stress corrosion cracking

Stress corrosion cracking occurs when tensile stress and a corrosive environment act together to cause cracking.

C276 demonstrates strong resistance to chloride-induced stress corrosion cracking and is also used in selected sour oilfield environments.

The actual material selection must still consider the applicable service qualification and environmental requirements.

6. Understanding Corrosion Test Data

When evaluating Hastelloy C276, buyers and engineers should understand how corrosion data is generated.

Manufacturers publish laboratory test results for different chemicals, concentrations and temperatures. These results can help engineers assess whether a material is suitable for a particular process.

However, laboratory corrosion rates are not universal performance guarantees.

Important variables include:

  • Chemical concentration
  • Operating temperature
  • Presence of impurities
  • Chloride and other halide content
  • Fluid velocity
  • Aeration and oxidation conditions
  • Exposure duration
  • Surface condition
  • Welded versus unwelded material

For critical applications, laboratory data should be reviewed by a corrosion or materials specialist, and field testing may be necessary before industrial use.

7. Where Is Hastelloy C276 Used?

The combination of corrosion resistance and useful mechanical properties makes C276 suitable for several industrial sectors.

Chemical processing

Used in selected reactors, heat exchangers, process columns, pumps and other equipment handling aggressive chemicals.

Pollution control

Used in selected flue-gas desulfurization systems, scrubbers and pollution-control equipment exposed to corrosive gases and chemical condensates.

Oil and gas

Considered for selected sour-service and corrosive process components, subject to the applicable service requirements and material qualification.

Pulp and paper

Used in selected chemical recovery and bleaching equipment where aggressive process chemicals are present.

Pharmaceutical and industrial processing

Used in selected process equipment where corrosion resistance and material reliability are important.

8. Hastelloy C276 Standards and Product Specifications

Different product forms of C276 are covered by different ASTM and ASME specifications.

Product formCommon specification
Rod and barASTM B574 / ASME SB574
Sheet, plate and stripASTM B575 / ASME SB575
Seamless pipe and tubeASTM B622 / ASME SB622
Welded pipe and tubeASTM B619 / ASME SB619
ForgingsASTM B564 / ASME SB564
FittingsASTM B366 / ASME SB366

The correct specification depends on the product form and purchase requirements. Always verify the applicable edition, supplementary requirements and acceptance criteria before ordering.

9. What Should Buyers Check Before Purchasing Hastelloy C276?

For industrial procurement, checking the grade alone is not sufficient. The complete material requirement should be documented.

Before placing an order, confirm:

  • Grade: Hastelloy C276 / UNS N10276
  • Product form: round bar, sheet, plate, pipe, tube or other required form
  • Applicable ASTM or ASME specification
  • Required diameter, thickness and length
  • Dimensional tolerances
  • Material condition
  • Chemical composition requirements
  • Mechanical testing requirements
  • Material Test Certificate (MTC)
  • Heat number and traceability
  • Additional inspection or testing, where required

For round-bar requirements, buyers can also use the round bar weight chart for preliminary material calculations.

10. Hastelloy C276 Supply Enquiries from Manan Steel & Metals

Manan Steel & Metals, established in 2007, supplies specialty metals and industrial steel products from Mumbai, India.

For Hastelloy C276 requirements, buyers can share the grade, product form, dimensions, quantity and applicable specification to help identify the correct material requirement.

Whether the requirement is for chemical-processing equipment, corrosion-resistant components or precision-machined industrial parts, providing complete technical details helps make procurement more efficient.

Contact Manan Steel & Metals

Frequently Asked Questions

1. What is the chemical composition of Hastelloy C276?

Hastelloy C276 contains nickel as the balance, with approximately 14.5–16.5% chromium, 15–17% molybdenum, 4–7% iron and 3–4.5% tungsten, along with controlled quantities of other elements.

2. What is the UNS number of Hastelloy C276?

The UNS number is N10276.

3. What is the Werkstoff number of Hastelloy C276?

The Werkstoff number is 2.4819.

4. What makes Hastelloy C276 corrosion resistant?

Its combination of nickel, chromium, molybdenum and tungsten contributes to resistance against several aggressive chemical environments, including selected chloride-bearing solutions and acids.

5. Is Hastelloy C276 resistant to hydrochloric acid?

C276 provides resistance in selected hydrochloric-acid conditions and can outperform many stainless steels in certain tested environments. Actual suitability depends on concentration, temperature and other operating conditions.

6. Is Hastelloy C276 suitable for high-temperature applications?

C276 has useful properties across a range of temperatures, but its suitability depends on the operating temperature, mechanical loading, corrosion environment and design code. It should not be selected solely on the basis of its corrosion resistance.

7. Which ASTM specification applies to Hastelloy C276 round bar?

ASTM B574 is the commonly referenced specification for C276 rod and bar. The applicable edition and purchase requirements should be confirmed.

8. What documents should buyers request for Hastelloy C276?

Buyers should specify an appropriate Material Test Certificate containing the material identification, chemical analysis, mechanical test results and heat traceability, along with any additional inspection documents required for the application.

Conclusion

Hastelloy C276 (UNS N10276) is a nickel-based alloy valued for its corrosion resistance in many demanding industrial environments. Its chromium, molybdenum and tungsten content contributes to resistance against pitting, crevice corrosion and selected acid environments.

For engineers and procurement teams, understanding the alloy’s chemical composition, mechanical properties and corrosion behaviour is essential before selecting it for industrial service.

When purchasing Hastelloy C276, verify the product specification, dimensions, material condition and certified test results to ensure the supplied material meets the intended requirements.


SEO Publishing Details

SEO Title: Hastelloy C276 Chemical Composition & Properties

Focus Keyword: Hastelloy C276 chemical composition

Secondary Keywords:

  • Hastelloy C276 mechanical properties
  • Hastelloy C276 corrosion resistance
  • UNS N10276 chemical composition
  • Alloy C276 properties
  • Hastelloy C276 density
  • Hastelloy C276 tensile strength
  • Hastelloy C276 specifications

URL Slug: hastelloy-c276-chemical-composition-mechanical-properties-corrosion-resistance

Meta Description: Understand Hastelloy C276 chemical composition, mechanical properties, corrosion resistance, physical characteristics and industrial applications of UNS N10276.

Featured Image Filename: hastelloy-c276-chemical-composition-properties.jpg

Image Alt Text: Hastelloy C276 UNS N10276 chemical composition and corrosion-resistant nickel alloy

Image Caption: Hastelloy C276 nickel-based alloy used in demanding corrosion-resistant industrial applications.

Internal Links

External Authority Links

Publishing Checklist

  • Use the article title as the only H1 heading.
  • Keep main sections as H2 and subsections as H3.
  • Add the focus keyword naturally in the title, introduction and relevant headings.
  • Add the featured image with the supplied alt text.
  • Keep internal links clickable.
  • Keep external links as normal clickable hyperlinks; do not mark them nofollow or sponsored.
  • Add the contact page link near the enquiry section.
  • Check that the article does not duplicate Blog 1.
  • Verify the final Rank Math analysis after publishing.